Reduced Remanence to Coercivity Increase Ratio of Pr11,76xDyxFe82B6 (x = 0; 1; 2; 3) Permanent Magnets

Nanang Sudrajat, A. Wisnu, Azwar Manaf

Research output: Contribution to journalConference articlepeer-review

Fingerprint

Dive into the research topics of 'Reduced Remanence to Coercivity Increase Ratio of Pr11,76xDyxFe82B6 (x = 0; 1; 2; 3) Permanent Magnets'. Together they form a unique fingerprint.